Why:
- Silicone oil spreads easily and forms ultra-thin films with low surface energy.
How to detect:
- Elevated water contact angle vs baseline
Corrective action:
- Eliminate silicone-based release agents or isolate processes
Stop dewetting, fish-eyes, and adhesion failures caused by silicone contamination and invisible residue with fast, quantitative surface testing.
Independent benchmarking and publication-based validation references.
Benchmark Validation
Our Contact angle and pendant‑drop surface tension methods have been benchmarked against KRÜSS DSA100E reference measurements.
See peer‑reviewed validationPublication Evidence
Our instruments are referenced in peer‑reviewed journals, theses, and conference publications
Browse the full citations listSpotted an issue in this summary? Send a correction request and our team will review it.
Correction Request
We work hard to keep this standards summary accurate and up to date. If you spot an error (wrong revision/year, missing requirement, incorrect interpretation, or broken link), tell us and we'll review it.
Contact us to report a correction