IPC-TM-650 Test Methods Manual, published by IPC as separate methods, each with its own revision. Methods on this page: 2.3.25D ROSE (November 2012), 2.3.28B ion chromatography (November 2012), 2.3.28.2 bare board cleanliness by ion chromatography (December 2009), 2.6.3.7 surface insulation resistance (March 2007), 2.6.3.5 bare board cleanliness by SIR (January 2004), 2.6.3.4A conformal coating moisture and insulation resistance (July 2003) and 2.4.28.1F solder mask tape adhesion (March 2007). See the IPC test methods listing.
Complements workflow. The Dropometer measures none of the quantities these TM-650 methods report: extract resistivity, ion content, insulation resistance or mask removed by tape. No current TM-650 method measures contact angle or surface tension. The Dropometer adds a water contact angle check for non ionic films before coating.
Contact angle range 10° to 175°, accuracy ±0.35°, display resolution 0.01°, from the Dropometer product specification.
The drop shape method is validated against a KRUSS DSA100E in two peer reviewed papers. See our validation publications.
A plating chemistry maker uses the Dropometer for contact angle and surface tension work. Read the case study. We have no published client study run alongside IPC-TM-650.
A water contact angle does not measure ionic cleanliness, insulation resistance or coating adhesion. Only the TM-650 tests do. Any link between an angle and those results comes from your own correlation study.